First Year Engineering is coming soon

We're still writing and reviewing the notes for every subject, and we'll open it when every subject is ready. Meanwhile you can practise aptitude, ask Aria about any subject, or see the branches that are ready.

Corrosion: mechanisms and types

Corrosion: mechanisms (electrochemical and dry/chemical), mixed-potential kinetics, and major types (uniform, galvanic, pitting, crevice, differential aeration, intergranular, erosion, SCC, microbial), with rate laws and exam-ready derivations and examples.

Drafted with Aria, reviewed by the AiCanCode.org team · Updated . How we write and check our notes. Spotted an error? Use Give Feedback at the bottom of the page.

Why it matters

Corrosion is the natural, gradual destruction of metals and alloys by chemical or electrochemical reaction with their environment, leading to loss of material, contamination, and failure of parts. Engineers must understand mechanisms and types to select materials, design joints, choose protective systems, estimate service life, and plan inspection in sectors like infrastructure, power plants, oil and gas, automotive, marine, and biomedical devices.

Key ideas

  • Chemical (dry) corrosion — direct reaction of a metal with a gas at high temperature (e.g., oxidation, sulphidation, carburization) without an electrolyte. Oxidation forms a surface oxide scale; kinetics often slow down with time due to diffusion through the scale.

  • Electrochemical (wet) corrosion — corrosion in the presence of an aqueous electrolyte. Microscopic anodic and cathodic areas form on the same metal surface or between dissimilar metals, creating galvanic cells.

  • Electrochemical theory of corrosion (exact statement)

    • “Electrochemical corrosion occurs by formation of anodic and cathodic sites on a metal in an electrolyte; metal dissolution occurs at anodes (oxidation), and a charge-balanced reduction occurs at cathodes. Ionic current flows through the electrolyte; electronic current flows through the metal, and the mixed potential where total anodic and cathodic currents are equal is the corrosion potential E_corr; the corresponding current density is the corrosion current density i_corr which governs the corrosion rate.” Assumptions: conductive electrolyte; electrical continuity through metal; at steady state no net charge builds; temperature and composition uniform enough for steady polarization behavior.
    • Typical half-reactions (iron in aerated neutral water):
      • Anode: Fe → Fe²⁺ + 2e⁻
      • Cathode: O2 + 2H2O + 4e⁻ → 4OH⁻ In acidic water: 2H⁺ + 2e⁻ → H2↑
  • Mixed-potential theory and polarization

    • Polarization is the shift of electrode potential from its equilibrium value when current flows, due to activation overpotential (charge transfer), concentration overpotential (mass transport limits), and ohmic drop (solution resistance).
    • Tafel behavior: at sufficiently high overpotentials for activation-controlled reactions, log current density varies linearly with overpotential for each half-reaction. Extrapolating anodic and cathodic Tafel lines to their intersection gives E_corr and I_corr.
    • Stern–Geary relation: near E_corr, the corrosion current density i_corr relates to the polarization resistance R_p: i_corr = B / R_p, where B depends on anodic and cathodic Tafel slopes.
  • Galvanic cells and series

    • Galvanic corrosion — when two dissimilar metals are electrically connected in an electrolyte, the more active (anodic) corrodes faster; the more noble (cathodic) is protected. Driving force depends on potential difference and area ratio (large cathode/small anode is severe).
    • Electrochemical series lists standard electrode potentials (activities at standard state). Galvanic series ranks alloys by corrosion potential in a specific environment (e.g., seawater), more predictive in practice.
  • Differential aeration and crevice effects

    • Differential aeration cell — areas with different dissolved oxygen become cathodic (high O2) and anodic (low O2), causing localized attack at oxygen-depleted spots (under deposits, gaskets, or in crevices).
    • Crevice corrosion — localized corrosion in shielded regions where stagnant solution leads to oxygen depletion, acidification, and chloride buildup, auto-accelerating metal dissolution.
  • Passivity

    • Passivation is the drastic reduction of corrosion rate due to formation of a thin, adherent, and protective oxide film on some metals (e.g., Al, Cr, Ti, stainless steels). Current–potential curves show an active–passive transition, a passive current plateau, and at high potentials possible transpassive dissolution.
  • Dry oxidation kinetics and protectiveness

    • At high temperature, many metals develop an oxide scale whose growth can be rate-limiting by diffusion of ions through the scale. Under diffusion control and constant conditions, oxide thickness x follows the parabolic law x² = k_p t + C.
    • Pilling–Bedworth ratio (P–B ratio) — “The ratio of the molar volume of oxide formed to the molar volume of metal consumed.” PB = (M_oxide/ρ_oxide) / (n·M_metal/ρ_metal), where n is number of metal atoms per formula unit of oxide. If PB < 1, oxide is porous and non-protective; if ~1–2, likely protective; if >>2, oxide may crack/spall.
  • Types of corrosion (with key features)

    • Uniform (general) corrosion — nearly even material loss across the surface; predictable; common in carbon steel in acids/alkalis.
    • Galvanic corrosion — between dissimilar metals/alloys in electrical contact in an electrolyte; severity increases with greater potential difference, higher conductivity, and unfavorable area ratio (small anode, large cathode).
    • Pitting corrosion — highly localized attack forming pits on passive metals in presence of halides (Cl⁻); initiation at inclusions/defects; autocatalytic due to pit chemistry (acidic, chloride-rich). Dangerous due to low weight loss but deep penetration.
    • Crevice corrosion — localized attack inside narrow gaps under gaskets, washers, lap joints due to differential aeration and chemistry changes.
    • Intergranular corrosion (IGC) — preferential attack along grain boundaries, often due to chromium carbide precipitation in sensitized austenitic stainless steels (depleting Cr at boundaries) or due to impurities at boundaries in other alloys.
    • Erosion–corrosion — accelerated attack due to relative motion of corrosive fluid removing protective films; depends on flow velocity, turbulence, particles/bubbles.
    • Stress corrosion cracking (SCC) — cracking due to combined effect of tensile stress (applied or residual) and a specific corrosive environment; slow crack growth leading to sudden failure. Examples: chloride SCC of austenitic stainless steels, caustic SCC of carbon steel.
    • Hydrogen damage (hydrogen embrittlement) — embrittlement or blistering due to absorbed atomic hydrogen; not always “corrosion” by mass loss but environment-induced cracking.
    • Microbiologically influenced corrosion (MIC) — corrosion affected by microorganisms (e.g., sulfate-reducing bacteria) changing local chemistry, producing H2S, or creating differential aeration.
    • High-temperature corrosion — oxidation, sulphidation in boilers, turbines, and furnaces; relates to dry corrosion mechanisms and oxide scale behavior.
  • What to draw for exam diagrams (describe clearly)

    • Electrochemical corrosion cell on a metal surface: draw a metal strip partially immersed in an electrolyte. Mark an anodic area (Fe → Fe²⁺ + 2e⁻) and a cathodic area (O2 + 2H2O + 4e⁻ → 4OH⁻). Show electron flow through the metal from anode to cathode and ion flow in the solution (Fe²⁺ away from anode; OH⁻ from cathode). Label E_corr and i_corr conceptually if plotting nearby.
    • Polarization (Evans) diagram: plot potential (vertical) vs log current density (horizontal). Draw anodic and cathodic Tafel lines; indicate intersection as E_corr, i_corr; show effect of cathodic limitation by oxygen reduction (plateau) and how lowering O2 shifts E_corr and i_corr.
    • Galvanic couple schematic: two dissimilar metals connected by a wire in an electrolyte; mark the anode (active) and cathode (noble), show electron flow anode→cathode and ionic current in solution; annotate effect of area ratio.
    • Pit geometry sketch: surface with small pit; indicate pit mouth, pit wall, aggressive pit chemistry (low pH, high Cl⁻), and passive surface around.
    • Oxidation kinetics: plot oxide thickness x vs t showing parabolic growth; annotate that slope decreases with time.

Formulas

  • CR = Δx / t — corrosion rate CR (m·s⁻¹) as thickness loss per time. Convert to mm·year⁻¹ when needed.
  • i_corr = B / R_p — Stern–Geary relation near E_corr: i_corr (A·m⁻²) is corrosion current density, R_p (Ω·m²) is polarization resistance; B (V) depends on Tafel slopes. Applies when linear polarization resistance method is valid.
  • B = (β_a · β_c) / (2.303 · (β_a + β_c)) — Stern–Geary constant from anodic (β_a) and cathodic (β_c) Tafel slopes (V·decade⁻¹). Use with i_corr = B/R_p.
  • x² = k_p · t + C — parabolic oxidation law for dry corrosion; x is oxide thickness (m), k_p is parabolic rate constant (m²·s⁻¹), C from initial condition. Applies when diffusion through oxide controls and conditions are steady.
  • PB = (M_oxide / ρ_oxide) / (n · M_metal / ρ_metal) — Pilling–Bedworth ratio, dimensionless; n is metal atoms per formula unit in the oxide (e.g., n = 2 for Fe2O3). Predicts oxide protectiveness qualitatively.
  • E = E° − (R · T / (n · F)) · ln(Q) — Nernst equation to estimate equilibrium potential (E, V) of a half-reaction with reaction quotient Q; R (J·mol⁻¹·K⁻¹), T (K), n, F as above. Useful to rationalize tendency but actual corrosion potential is at mixed conditions.

Worked examples

  1. Uniform corrosion rate from mass loss (coupon test) Given: A steel plate coupon, both faces exposed. Area A = 10 cm × 10 cm on each side → total area = 2 × (0.10 m × 0.10 m) = 0.02 m². Exposure time t = 30 days. Mass loss m = 0.520 g. Density of steel ρ = 7.87 g·cm⁻³. Steps:
  1. Convert units: m = 0.520 g = 5.20 × 10⁻⁴ kg; ρ = 7.87 g·cm⁻³ = 7870 kg·m⁻³; t = 30 days = 30 × 24 × 3600 = 2,592,000 s.
  2. Thickness loss: Δx = m / (ρ · A) = (5.20 × 10⁻⁴ kg) / (7870 kg·m⁻³ × 0.02 m²) = 3.304 × 10⁻⁶ m.
  3. Convert to annual corrosion rate: CR_year = Δx × (365/30) per year = 3.304 × 10⁻⁶ m × 12.1667 = 4.017 × 10⁻⁵ m·year⁻¹ = 0.0402 mm·year⁻¹. Answer: The corrosion rate is 0.040 mm·year⁻¹ (approximately uniform).
  1. Thickness loss from corrosion current density (Faraday’s law) Given: Iron in neutral aerated water with measured corrosion current density i_corr = 10 μA·cm⁻². Estimate thickness loss in one year. Data: i_corr = 10 μA·cm⁻² = 0.1 A·m⁻²; t = 1 year = 31,536,000 s; M_Fe = 55.845 g·mol⁻¹ = 0.055845 kg·mol⁻¹; n = 2 (Fe → Fe²⁺ + 2e⁻); F = 96,485 C·mol⁻¹; ρ_Fe = 7870 kg·m⁻³. Steps:
  1. Mass loss per unit area by Faraday’s law: m/A = (i_corr · t · M) / (n · F) = (0.1 A·m⁻² × 31,536,000 s × 0.055845 kg·mol⁻¹) / (2 × 96,485 C·mol⁻¹) = 9.13 × 10⁻¹ kg·m⁻² (approximately 0.913 kg·m⁻²).
  2. Thickness loss: Δx = (m/A) / ρ = (0.913 kg·m⁻²) / (7870 kg·m⁻³) = 1.160 × 10⁻⁴ m.
  3. Convert to mm·year⁻¹: 1.160 × 10⁻⁴ m = 0.116 mm. Answer: The annual thickness loss is 0.116 mm·year⁻¹ for i_corr = 10 μA·cm⁻².

Check: Using the combined formula Δx = (i · t · M) / (n · F · ρ) directly gives 1.16 × 10⁻⁴ m·year⁻¹, consistent with the step-by-step result. Rule of thumb: for iron, 1 μA·cm⁻² ≈ 0.0116 mm·year⁻¹, so 10 μA·cm⁻² ≈ 0.116 mm·year⁻¹.

  1. Long-answer model: Explain galvanic corrosion with conditions, mechanism, examples, and prevention Definition: Galvanic corrosion is the accelerated corrosion of a more active metal (anode) when electrically connected to a more noble metal (cathode) in an electrolyte. Conditions:
  • Two dissimilar metals/alloys with sufficiently different corrosion potentials in the same environment.
  • Electrical contact between the metals (direct or via a wire).
  • Common electrolyte providing ionic conductivity between the metals. Mechanism:
  • The metals and electrolyte form a galvanic cell. The metal with lower potential (more active) becomes the anode and dissolves (M → Mⁿ⁺ + ne⁻). The noble metal is the cathode where a reduction reaction occurs (often oxygen reduction or hydrogen evolution). Electrons flow through the metallic path from anode to cathode; ionic current completes the circuit in the electrolyte. The mixed potential shifts such that the total anodic current equals the total cathodic current. A large cathode-to-anode area ratio increases anodic current density, making attack on the small anode severe. Examples:
  • Carbon steel (anode) coupled to copper (cathode) in seawater: steel corrodes rapidly near the junction.
  • Aluminum rivets (anode) with stainless steel sheets (cathode) in marine atmosphere: rivets pit and loosen.
  • Zinc sacrificial anodes (deliberate anode) protecting steel hulls: zinc dissolves, steel is cathodically protected. Prevention/mitigation:
  • Avoid dissimilar metal contact in the same electrolyte; use electrically insulating gaskets, sleeves, or coatings to break the circuit.
  • Choose metals close in the galvanic series for the given environment.
  • Control area ratio: avoid small anodes coupled to large cathodes; if unavoidable, coat the cathode or increase anode area.
  • Reduce electrolyte conductivity or exclude the electrolyte (sealing, drying).
  • Apply cathodic protection (sacrificial anodes or impressed current) to shift potential and suppress anodic dissolution on the structure.
  • Use corrosion inhibitors compatible with the system.

Common mistakes

  • Ignoring area effects in galvanic couples; not noting that a small anodic area with a large cathodic area is most dangerous.
  • Using standard electrode potentials (electrochemical series) to predict galvanic behavior in seawater without considering the galvanic series for that environment.
  • Calculating thickness loss without converting units (e.g., g·cm⁻³ to kg·m⁻³, μA·cm⁻² to A·m⁻²) or forgetting that both sides of a coupon may be exposed.
  • Applying parabolic oxidation law when the scale is spalling or porous; not checking assumptions before using x² = k_p t.
  • Confusing passivation (low current) with immunity (thermodynamic stability). Passive metals can still suffer pitting/crevice attack.

For your exam

  • Diagrams: electrochemical cell on a corroding surface; Evans diagram showing E_corr and i_corr; galvanic couple with area ratio; pit schematic; oxide thickness vs time (parabolic law). Label all arrows, reactions, and axes.
  • Derivations/logic steps often asked:
    • Derive Stern–Geary relation (state result and show linearization near E_corr) or use it to compute i_corr from R_p and B.
    • Show how Tafel extrapolation gives E_corr and i_corr from anodic and cathodic branches.
    • Derive parabolic oxidation law assuming diffusion control through a planar oxide film (flux proportional to concentration gradient; mass gain proportional to flux; integrate to x² ∝ t).
    • Express PB ratio and interpret protectiveness ranges.
  • Numericals: convert i_corr to corrosion penetration rate using Faraday’s law and density; compute thickness loss from mass-loss test; convert units to mm·year⁻¹ in SI.
  • Full-marks answers include: clear definitions, assumptions, neat labeled diagrams as described, correct formulas with symbols and units, stepwise calculations with units, and a brief remark on applicability/limitations.

Quick check

  1. State the difference between electrochemical and chemical corrosion with one example each.
  2. Why is a small area of aluminum rivet attached to a large stainless-steel sheet in seawater at risk? Name the type of corrosion and the reason.
  3. Write the Pilling–Bedworth ratio formula and explain what PB < 1 implies. Answers: 1) Electrochemical (wet) corrosion needs an electrolyte and anodic/cathodic reactions, e.g., rusting of iron in aerated water; chemical (dry) corrosion is direct high-temperature reaction with gases, e.g., oxidation of hot steel in air. 2) Galvanic corrosion; the aluminum is the small anode coupled to a large noble cathode, giving high anodic current density and rapid localized attack. 3) PB = (M_oxide/ρ_oxide)/(n·M_metal/ρ_metal); PB < 1 means the oxide volume is too small to cover the metal, so the scale is porous/non-protective and corrosion continues.

Finished this topic? Mark it so your progress, study plan and readiness keep up.

Stuck on something here?