Engineering Materials and Manufacturing Processes — formula sheet
Mechatronics Engineering · GATE ME · SI units. Drafted with Aria, checked by the AiCanCode.org team.
Crystal structure, defects and mechanical properties of metals
ρ = n·A / (a³·N_A)— theoretical density (kg/m³ or g/cm³); n: atoms per unit cell (SC 1, BCC 2, FCC 4); A: atomic mass (g/mol); a: lattice parameter; N_A = 6.022 × 10²³ mol⁻¹; cubic crystals.a = 4r/√3(BCC),a = 2√2·r(FCC),a = 2r(SC) — r: atomic radius; atoms touch along the body diagonal (BCC) or face diagonal (FCC).APF = n·(4/3)·π·r³ / a³— atomic packing factor: SC 0.52, BCC 0.68, FCC and HCP 0.74.σ_y = σ₀ + k·d^(−1/2)— Hall–Petch: σ_y yield strength (MPa); σ₀ friction stress (MPa); k locking parameter (MPa·m^0.5); d grain diameter (m).σ = F/A₀,ε = ΔL/L₀,E = σ/ε— engineering stress (Pa), strain (dimensionless), Young's modulus (Pa); E applies in the elastic region only.σ_T = σ·(1 + ε),ε_T = ln(1 + ε)— true stress and true strain; valid up to the onset of necking.U_r = σ_y² / (2E)— modulus of resilience (J/m³).
Iron-carbon diagram, steels and cast irons
- Key points: eutectoid 727 °C, 0.76 % C (γ → α + Fe₃C, pearlite); eutectic 1147 °C, 4.3 % C (L → γ + Fe₃C, ledeburite); peritectic 1495 °C, 0.17 % C (L + δ → γ); max C in ferrite 0.022 %, in austenite 2.14 %; cementite 6.67 % C.
W_β = (C₀ − C_α) / (C_β − C_α)— lever rule: mass fraction of phase β in a two-phase field; C₀ alloy composition, C_α and C_β tie-line end compositions (wt%).W_pearlite = (C₀ − 0.022) / (0.76 − 0.022)— hypoeutectoid steel just below 727 °C.W_pearlite = (6.67 − C₀) / (6.67 − 0.76)— hypereutectoid steel just below 727 °C.CE = C + (Si + P)/3— carbon equivalent of cast iron (wt%); CE ≈ 4.3 is eutectic.CE_IIW = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15— carbon equivalent for weldability of steels (wt%); higher CE means greater risk of hydrogen cracking and need for preheat.
Heat treatment and surface hardening of steels
x ∝ √(D·t)— case depth x (m) at fixed temperature; D diffusion coefficient (m²/s); t time (s). Doubling depth needs four times the time.(C_s − C_x) / (C_s − C₀) = erf( x / (2·√(D·t)) )— Fick's second-law solution for carburising a semi-infinite solid at constant surface carbon C_s; C₀ initial carbon; C_x carbon at depth x (wt%).D = D₀·exp(−Q / (R·T))— D₀ (m²/s), Q activation energy (J/mol), R = 8.314 J/(mol·K), T in K; D₀ and Q from the data book.δ = 503·√( ρ / (μ_r·f) )— induction skin depth (m); ρ resistivity (Ω·m); μ_r relative permeability (1 above the Curie point); f frequency (Hz).
Smart materials: piezoelectric, shape memory alloys
D = d·T + ε^T·E— direct piezoelectric effect: D electric displacement (C/m²); d charge coefficient (C/N); T stress (Pa); ε^T = ε_r·ε₀ permittivity (F/m), ε₀ = 8.854 × 10⁻¹² F/m; E field (V/m).S = s^E·T + d·E— converse effect: S strain; s^E compliance (m²/N).Q = d₃₃·F— charge (C) from axial force F (N) on a thickness-mode element.C = ε^T·A / t,V = Q / C— element capacitance (F), open-circuit voltage (V); A electrode area (m²), t thickness (m).g₃₃ = d₃₃ / ε₃₃^T,V = g₃₃·σ·t— voltage coefficient (V·m/N).Δ = n·d₃₃·V— free stroke (m) of an n-layer stack driven at V volts per layer.k² = d² / (s^E·ε^T)— electromechanical coupling factor.F = σ_r·π·d_w² / 4,δ = ε_r·L— SMA wire force (N) and stroke (m); σ_r recovery stress (Pa) and ε_r design recoverable strain from supplier data; L active length (m).
Sand casting: patterns, moulds, gating and risers
Pattern size = (casting size + machining allowance) × (1 + shrinkage allowance)— allowances from the foundry data book; draft is added separately.v = √(2·g·h)— velocity at the sprue base (m/s); h effective head (m); g = 9.81 m/s².A_top·√h_top = A_bottom·√h_bottom— sprue taper from continuity to avoid aspiration.t_f = V / (A_g·√(2·g·h_t))— mould filling time (s), top gating; V mould volume (m³); A_g gate (choke) area (m²); h_t sprue height (m).t_f = (A_m / A_g)·(2 / √(2·g))·(√h_t − √(h_t − h_m))— filling time, bottom gating; A_m mould cross-section (m²); h_m mould height (m).M = V / A,M_riser ≥ 1.2·M_casting— casting modulus (m); riser sized so it freezes after the casting (modulus method).
Solidification time and special casting processes
t_s = B·(V/A)ⁿ— Chvorinov's rule: t_s solidification time (s); B mould constant (s/m², for n = 2); V volume (m³); A cooling surface area (m²); n ≈ 2.t₂ / t₁ = (M₂ / M₁)²— ratio of solidification times for the same metal and mould.d = k·√t— solidified skin thickness (m) after time t (s); k solidification constant (m/s^0.5).G = ω²·R / g,N = (60 / 2π)·√(G·g / R)— centrifugal casting: G-factor (dimensionless); ω (rad/s); R inner radius of casting (m); N (rpm).
Bulk forming: forging, rolling, extrusion and drawing
ε = ln(A₀/A_f) = ln(h₀/h_f)— true strain; plane-strain rolling uses thickness.σ̄_f = K·εⁿ / (1 + n)— average flow stress (Pa); K strength coefficient (Pa); n strain-hardening exponent.Δh_max = μ²·R,L = √(R·Δh)— maximum draft (m) and projected contact length (m) in rolling; R roll radius (m); μ friction coefficient.F = σ̄_f·w·L— roll separating force (N), friction neglected; w strip width (m).T = 0.5·F·L(per roll),P = 2π·N·F·L / 60(both rolls) — torque (N·m) and power (W); N roll speed (rpm).p_avg = σ_f·(1 + 2μr / (3h)),F = p_avg·π·r²— open-die upsetting of a cylinder of radius r and height h with sliding friction.σ_d = σ̄_f·ln(A₀/A_f),F_d = σ_d·A_f— ideal (frictionless) wire or rod drawing stress and force; maximum ideal reduction 63.2 % (σ_d = σ_f).p = σ̄_f·ln R,F = p·A₀— ideal extrusion pressure (Pa) and force (N); R = A₀/A_f extrusion ratio; A₀ billet area.
Sheet metal operations: blanking, bending and deep drawing
F_s = L·t·τ— blanking or punching force (N); L cut perimeter (m); t thickness (m); τ shear strength (Pa).c = a·t— radial clearance per side (m); a allowance from the data book. Blanking: die = blank size, punch = die − 2c. Punching: punch = hole size, die = punch + 2c.BA = α·(R + K·t)— bend allowance (m); α bend angle (rad); R inside bend radius (m); K neutral-axis factor (≈ 0.33 for R < 2t, ≈ 0.5 for R ≥ 2t).F_b = K_b·σ_u·w·t² / D— bending force (N); K_b die factor (≈ 1.33 for V-die, 0.33 for wiping die); σ_u UTS (Pa); w bend length (m); D die opening (m).D = √(d² + 4·d·h)— blank diameter (m) for a cylindrical cup of diameter d and height h, sharp corners, thickness constant.DR = D / d,r = (D − d) / D— drawing ratio (limit about 2.0 for first draw) and reduction.F_d = π·d·t·σ_u·(D/d − 0.7)— empirical deep-drawing force (N).
Powder metallurgy
ρ_rel = ρ / ρ_th,Porosity = 1 − ρ / ρ_th— relative density and porosity; ρ_th theoretical (pore-free) density.m = ρ_g·V_g = ρ_s·V_s— mass is conserved between green (g) and sintered (s) compacts.Volumetric shrinkage = 1 − ρ_g / ρ_s,Linear shrinkage = 1 − (ρ_g / ρ_s)^(1/3)— isotropic shrinkage on sintering.F = p·A— press force (N) for compaction pressure p (Pa) on projected area A (m²).
Arc, gas and resistance welding; heat input
H = η·V·I / v— net heat input per unit length (J/m); η arc (heat-transfer) efficiency, typically 0.6–0.9 depending on process; V arc voltage (V); I current (A); v travel speed (m/s).H (kJ/mm) = 60·V·I / (1000·S)— gross heat input with S in mm/min (multiply by η for net).V = A + B·l— arc voltage (V) versus arc length l (mm); A and B from the power-source data.V = V_o − (V_o / I_s)·I— linear drooping power-source characteristic; V_o open-circuit voltage; I_s short-circuit current.Q = I²·R·t— resistance-welding heat (J); R contact plus bulk resistance (Ω); t weld time (s).η_m = u·A_w·v / (η·V·I)— melting efficiency; u energy to melt unit volume (J/m³); A_w weld bead cross-section (m²).
Solid-state welding, brazing and soldering
T = (2/3)·μ·F·R— friction torque (N·m) on a solid circular face of radius R (m) under axial force F (N), uniform pressure.P = T·ω,ω = 2πN / 60— friction-welding power (W).P_joint = τ_f·A_lap— strength of a brazed or soldered lap joint (N); τ_f filler shear strength (Pa); A_lap overlap area (m²).L = σ_t·t / τ_f— lap length (m) for the joint to be as strong as the sheet of thickness t and tensile strength σ_t.Q = m·c·ΔT— sensible heat (J) to bring a part to brazing temperature (add latent heat if any metal melts).
Mechanics of orthogonal cutting and Merchant's circle
r = t / t_c = V_c / V = l_c / l— chip thickness ratio (< 1).tan φ = r·cos α / (1 − r·sin α)— shear angle φ; α rake angle.F = F_c·sin α + F_t·cos α,N = F_c·cos α − F_t·sin α,μ = tan β = F / N— friction force and normal force on the rake face; β friction angle.F_s = F_c·cos φ − F_t·sin φ,F_n = F_c·sin φ + F_t·cos φ— shear-plane forces.F_c = R·cos(β − α),F_t = R·sin(β − α),F_s = R·cos(φ + β − α)— R resultant tool force.A_s = b·t / sin φ,τ_s = F_s / A_s— shear-plane area and shear stress; b width of cut.2φ + β − α = 90°— Merchant's shear-angle relation (minimum energy).V_c = V·sin φ / cos(φ − α),V_s = V·cos α / cos(φ − α)— chip and shear velocities.γ = cot φ + tan(φ − α)— shear strain.P = F_c·V,u = F_c / (b·t)— cutting power (W) and specific cutting energy (J/m³).
Tool wear, tool life and machinability
V·T^n = C— Taylor's equation: V cutting speed (m/min); T tool life (min); n exponent (dimensionless, typically about 0.1–0.15 HSS, 0.2–0.3 carbide, 0.4–0.6 ceramic; take from test data); C speed for 1 min life (m/min). Valid for one tool–work pair, fixed feed and depth.n = ln(V₂/V₁) / ln(T₁/T₂)— exponent from two tests.T₂ = T₁·(V₁/V₂)^(1/n)— tool life at a new speed.V·T^n·f^a·d^b = C— extended Taylor equation; f feed (mm/rev), d depth of cut (mm), a and b empirical.T_c = (1/n − 1)·(t_c + C_t/C_m)— tool life for minimum cost; t_c tool-change time (min); C_t cost per cutting edge; C_m machine-and-labour cost rate per min.T_p = (1/n − 1)·t_c— tool life for maximum production rate.Machinability index (%) = (V_test / V_reference) × 100— speeds for the same tool life.
Turning, milling, drilling and grinding; machining time
N = 1000·V / (π·D)— spindle speed (rpm); V (m/min); D (mm).t = (L + A + O) / (f·N)— time per pass (min) in turning or drilling; L length of cut, A approach, O over-travel (mm); f feed (mm/rev).MRR = π·D_avg·d·f·N ≈ 1000·V·f·d— turning MRR (mm³/min); d depth of cut (mm); D_avg mean diameter (mm).t = (D/2) / (f·N)— facing time (min) from outside to centre at constant N.Drill tip allowance = (D/2)·cot(θ/2)— θ point angle (118° gives about 0.3D).MRR = (π·D²/4)·f·N— drilling into solid (mm³/min).f_m = f_z·Z·N— milling table feed (mm/min); f_z feed per tooth (mm); Z number of teeth.t = (L + A + O) / f_m,A = √(d·(D − d))— milling time (min) and slab-milling approach (mm); D cutter diameter.MRR = w·d·f_m— milling MRR (mm³/min); w width of cut (mm).P = u·MRR— cutting power (W) with u specific cutting energy (J/mm³, data book) and MRR in mm³/s.
Jigs and fixtures
3 + 2 + 1 = 6— the 3-2-1 principle: 3 locators on the primary face, 2 on the secondary, 1 on the tertiary arrest all six degrees of freedom.W ≥ n·F / (k·μ)— clamping force (N) to resist a sliding force F (N) by friction alone; μ friction coefficient; k number of friction interfaces (1 or 2); n factor of safety (about 1.5–3). Prefer directing cutting forces into fixed locators.h = D / (2·sin(α/2))— height of a cylinder's axis above the V-block vertex; D diameter; α included V angle.Δh = ΔD / (2·sin(α/2))— vertical location error of the axis due to diameter variation ΔD.
Non-traditional machining: EDM, ECM, USM, LBM, AJM
ṁ = η·I·A / (v·F)— ECM mass removal rate (g/s); η current efficiency; I current (A); A atomic mass (g/mol); v valency; F = 96 485 C/mol.Q = η·I·A / (v·F·ρ)— ECM volumetric MRR (cm³/s); ρ density (g/cm³).f = η·J·A / (v·F·ρ)— ECM equilibrium tool feed (cm/s); J current density (A/cm²).A/v (alloy) = 1 / Σ(x_i·v_i/A_i)— effective electrochemical equivalent of an alloy; x_i mass fraction.V_c = V₀·(1 − e^(−t/RC))— EDM RC (relaxation) circuit capacitor voltage while charging; V₀ supply voltage; R (Ω); C (F).E_s = ½·C·V_d²,P = E_s / t_c— energy per spark (J) at discharge voltage V_d, and average power (W) for charging time t_c.v_max = 2·π·f·a— USM peak tool velocity (m/s); f frequency (Hz); a amplitude (m).Power density = P / (π·d²/4)— LBM power density (W/m²); P beam power (W); d spot diameter (m).
Plastic processing: injection moulding and extrusion
F_clamp = p_c·A_p— clamping force (N); p_c average cavity pressure (Pa, typically 20–100 MPa by material); A_p projected area of part plus runners (m²).t_c = (s² / (π²·α))·ln[(4/π)·(T_m − T_w)/(T_e − T_w)]— cooling time (s) of a plate cooled from both faces; s wall thickness (m); α thermal diffusivity (m²/s, about 1 × 10⁻⁷ for polymers); T_m melt, T_w mould wall, T_e ejection temperature.D_c = D_p / (1 − S) ≈ D_p·(1 + S)— cavity dimension from part dimension and fractional shrinkage S (supplier data).Q_d = ½·π²·D²·N·h·sin φ·cos φ— extruder drag flow (m³/s); D screw diameter (m); N speed (rev/s); h channel depth (m); φ helix angle (17.66° for square pitch).Q_p = π·D·h³·sin²φ·Δp / (12·η·L)— pressure back-flow (m³/s); Δp die head pressure (Pa); η melt viscosity (Pa·s); L metering length (m).Q = Q_d − Q_p— net extruder output; the operating point is where it meets the die characteristic Q = K_s·Δp.